Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
23.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |