Physical Properties Metric English Comments
Melt Flow 22.4 g/10 min

@Load 0.325 kg,
Temperature 190 °C
22.4 g/10 min

@Load 0.716 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Fusabond® P353 Polymer Modifier
DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun..