Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 - 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 - 20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10 - 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 - 20 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 50; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 16 - 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 - 20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4052V (52418) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10 - 20 g/10 min @Load 5.00 kg, Temperature 230 °C |
10 - 20 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |