Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.1 - 2.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 - 2.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |