Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19.35 g/10 min @Load 2.16 kg, Temperature 230 °C |
19.35 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 15 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |