Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 72 - 160 g/10 min @Load 21.6 kg, Temperature 190 °C |
72 - 160 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio 30-50; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |