Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 15.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 15.0 g/10 min

@Load 21.6 kg,
Temperature 230 °C
15.0 g/10 min

@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinelec CCB2095 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Ape..
Melt Flow 15.0 g/10 min

@Load 21.6 kg,
Temperature 200 °C
15.0 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Sinelec CCB2095 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Forms: Pellets Processing Method: Injection MethodInformation Provided by Teknor Ape..