Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 135 g/10 min @Load 21.6 kg, Temperature 190 °C |
135 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |