Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 132 g/10 min @Load 5.00 kg, Temperature 275 °C |
132 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Melt Flow | 132 g/10 min @Load 5.00 kg, Temperature 275 °C |
132 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |