Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.4 g/10 min @Load 2.16 kg, Temperature 260 °C |
13.4 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region. |