Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.026 g/10 min @Load 5.00 kg, Temperature 200 °C |
13.026 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |