Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.8 g/10 min @Load 3.80 kg, Temperature 260 °C |
12.8 g/10 min @Load 8.38 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |