Melt Flow 9.0 - 12.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 - 12.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 - 12.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 - 12.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer