Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Melt Flow | 112.2 g/10 min @Load 5.00 kg, Temperature 300 °C |
112.2 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |