Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 10.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, ..
Melt Flow 10.1 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10.1 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Procedure A; ASTM D1238
Diamond Polymers ABS VP-11 ELG
Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc.