Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.58 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.58 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Braskem HF0144 High Density Polyethylene Blends for irrigation pipes.Information provided by Braskem. |