Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.32 g/10 min @Load 5.00 kg |
0.32 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total 2285 HDPE Bimodal Film Resin Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals. |
|||
Melt Flow | 0.32 g/10 min @Load 5.00 kg |
0.32 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |