Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.23 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.23 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Melt Flow | 0.23 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |