Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.21 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.21 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer GF4950HS resin is a high-density polyethylene (HDPE), bimodal copolymer offering a combination of good processability and environmental stress crack resistance (ESCR). It is thus recommended for the.. |