Polymer Property : Oxygen Transmission Rate = 8.37 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 130 cc/m²/day

@Thickness 0.0200 mm
8.37 cc/100 in²/day

@Thickness 0.000787 in
1 bar; ISO 15 105-2
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..