Physical Properties Metric English Comments
Oxygen Transmission Rate >= 1000 cc/m²/day
>= 64.4 cc/100 in²/day
25°C, 1.0 µm, 0% RH
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop..