Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 6200 cc/m²/day | 399 cc/100 in²/day | Cast Film at 1.25 mil; ASTM D-3985 |
Chevron Phillips MarFlex® 4553 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceLow coefficient of friction Applications: .. |