Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 6100 cc/m²/day | 393 cc/100 in²/day | Blown Film at 1.25 mil; ASTM D-3985 |
Chevron Phillips MarFlex® 4571 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceHigh coefficient of friction Applications:.. |