Physical Properties Metric English Comments
Oxygen Transmission Rate 850 cc/m²/day

@Thickness 0.0450 mm
54.7 cc/100 in²/day

@Thickness 0.00177 in
1 bar; ISO 15 105-2
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..