Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 7140 cc/m²/day | 460 cc/100 in²/day | ASTM D1922 |
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets A.. |