Polymer Property : Oxygen Transmission Rate = 370 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 370 cc/m²/day
23.8 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® L 25 G nat 6011 PA12
Product Description: Grilamid L 25 G natural 6011 is a high viscosity, lubricated polyamide 12. This product has the following features: Very tastelessHigh toughness, even at low temperaturesGood re..
Oxygen Transmission Rate 370 cc/m²/day
23.8 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® L 25 nat PA12
Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go..