Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 49.7 cc/m²/day @Temperature 23.0 °C |
3.20 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |