Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 3500 cc/m²/day | 225 cc/100 in²/day | At 25°C/0% RH/1 bar; ASTM D3985 |
Borealis Borstar® FB2310 LLDPE for Film Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Oxygen Transmission Rate | 3500 - 5000 cc/m²/day | 225 - 322 cc/100 in²/day | Average value: 4500 cc/m²/day Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |