Oxygen Transmission Rate 0.0931 - 2100 cc/m²/day
0.00600 - 135 cc/100 in²/day
Average value: 375 cc/m²/day Grade Count:74
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..