Physical Properties Metric English Comments
Oxygen Transmission Rate <= 20.0 cc/m²/day
<= 1.29 cc/100 in²/day
23°C; 50% RH; ASTM F1927
OCTAL DPET™/PE Lock-Up Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Oxygen Transmission Rate <= 20.0 cc/m²/day
<= 1.29 cc/100 in²/day
23°C; 50% RH; ASTM F1927
OCTAL DPET™/PE Peelable Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.