Polymer Property : Oxygen Transmission Rate = 1705 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 1705 cc/m²/day
109.8 cc/100 in²/day
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin
Film Properties.Data provided by the manufacturer.
Oxygen Transmission Rate 1705 cc/m²/day
109.8 cc/100 in²/day
NOVA Chemicals Sclair® 19H Homopolymer HDPE Film Resin
Features: High stiffnessGood processability Low gel Applications: BlendingCo-extrusionInformation provided by Nova Chemicals