Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 202 - 233 cc/m²/day | 13.0 - 15.0 cc/100 in²/day | 25°C / 0%RH; ASTM D3985 |
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
(discontinued **) Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell. |