Polymer Property : Oxygen Transmission Rate = 15.0 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 15.0 cc/m²/day
0.966 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
ExxonMobil Bicor® 70 PXS OPP Film
Product Description: Bicor PXS is one-side sealable, PVdC-coated OPP film designed for use as the inside sealant web in laminations.Availability: Latin America, North America and South AmericaKey Fe..