Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 0.470 cc/m²/day | 0.0303 cc/100 in²/day | 50°F (10°C) / 0%RH; ASTM D3985 |
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro.. |
|||
Oxygen Transmission Rate | 0.470 cc/m²/day | 0.0303 cc/100 in²/day | 73°F (23°C) / 65%RH; ASTM D3985 |
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat.. |