Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 3.10 cc/m²/day | 0.200 cc/100 in²/day | 73°F (23°C) / 65%RH; ASTM D3985 |
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |