Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 1.55 cc/m²/day | 0.0998 cc/100 in²/day | 73°F - 65%RH; ASTM D3985 |
Honeywell Capran® NyLid™ OMBS-100M Nylon Lidding Film
(discontinued **) Description: Capran® NyLid™ OMBS-100M is a mono-axially oriented, co-extruded Nylon 6/EVOH/Nylong 6 clear film with a print/lamination receptive coating having excellent gas barrier through a broa.. |
|||
Oxygen Transmission Rate | 1.55 cc/m²/day | 0.0998 cc/100 in²/day | 73°F - 0%RH; ASTM D3985 |
Honeywell Capran® NyLid™ OMBS-100M Nylon Lidding Film
(discontinued **) Description: Capran® NyLid™ OMBS-100M is a mono-axially oriented, co-extruded Nylon 6/EVOH/Nylong 6 clear film with a print/lamination receptive coating having excellent gas barrier through a broa.. |
|||
Oxygen Transmission Rate | 1.55 cc/m²/day | 0.0998 cc/100 in²/day | 73°F (23°C) / 65%RH; ASTM D3985 |
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |