Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 6000 - 9500 g/m²/day @Temperature 38.0 - 38.0 °C |
386 - 612 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 7750 g/m²/day Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |