Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 9.30 - 9.30 g/m²/day @Temperature 38.0 - 38.0 °C |
0.599 - 0.599 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 9.30 g/m²/day Grade Count:1 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |