Physical Properties Metric English Comments
Water Vapor Transmission 7400 g/m²/day
477 g/100 in²/day
ASTM E-96BW
GRECO ISOTHANE 1690AE Polyether TPU Resin
ISOTHANE 1600 series products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be e xtruded and blowed.Inf..