Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 104 g/m²/day | 6.70 g/100 in²/day | JIS Z0208 |
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 .. |