Polymer Property : Water Vapor Transmission = 515 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 8000 g/m²/day
515 g/100 in²/day
38%, 90%RH; DIN 53.122
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan..