Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 420 g/m²/day | 27.0 g/100 in²/day | 50% RH; ASTM E96B |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Water Vapor Transmission | 420 g/m²/day | 27.0 g/100 in²/day | ASTM E96B |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Water Vapor Transmission | 420 - 9000 g/m²/day | 27.0 - 580 g/100 in²/day | Average value: 3770 g/m²/day Grade Count:7 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |