Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 388 - 465 g/m²/day | 25.0 - 29.9 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl.. |