Physical Properties Metric English Comments
Water Vapor Transmission 1.00 - 3.00 g/m²/day
0.0644 - 0.193 g/100 in²/day
38°C at 90% RH, On 300 micron film; ISO 1195
Total Lacqrene® 9218 Polystyrene  (discontinued **)
LACQRENE® 9218 is a polystyrene modified with polyethylene. This combination gives a high level of stress crack resistance with excellent mechanical properties and good abrasion resistance. This ..