Polymer Property : Water Vapor Transmission = 2.51 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 39.0 g/m²/day
2.51 g/100 in²/day
ASTM F372
Eastman Eastobond 19411 Copolyester, Film
Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so..
Water Vapor Transmission 39.0 g/m²/day
2.51 g/100 in²/day
ASTM F372
Eastman Eastobond 19412 Copolyester, Film
Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob..