Polymer Property : Water Vapor Transmission = 2.50 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 2.50 g/m²/day
0.161 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 110 AXT OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur..
Water Vapor Transmission 2.50 g/m²/day
0.161 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 70 HBS-2 OPP Film
Product Description: Bicor HBS-2 is a one-side sealable, one-side high barrier PVdC-coated OPP film designed for use as the inside sealant web in high-barrier laminations.Availability: Latin America..