Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 171 - 202 g/m²/day | 11.0 - 13.0 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Water Vapor Transmission | 171 - 202 g/m²/day | 11.0 - 13.0 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |