Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.500 - 15.5 g/m²/day | 0.0322 - 0.998 g/100 in²/day | Average value: 6.87 g/m²/day Grade Count:21 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |