Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 9.30 - 12.4 g/m²/day | 0.599 - 0.799 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |