Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0497 - 10.9 g/m²/day | 0.00320 - 0.702 g/100 in²/day | Average value: 2.99 g/m²/day Grade Count:133 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |